Preparation

  • Each part is pre-treated in our five-stage washer system that cleans, degreases and etches for maximum powder coating adhesion.
  • Parts that with an old, existing finish are and sandblasted and, when necessary, hand sanded to provide a clean surface for new powder.

Coating

  • Pigment and resin are electrostatically charged and sprayed onto each part from two manually operated spray guns.
  • The parts are then “cured” in our high-temperature ovens—anywhere from 180C degrees to 220C degrees, depending on a parts curing needs. As the finish cures, the powder fuses to a consistent, durable finish that will last for years.